Study on basic wood properties of critically endangered species Syzygium album

Syzygium album is a critically endangered species, and the wood basic properties haven’t been reported. Therefore, this paper analyzes the wood from the anatomical characteristics, physical properties, and secondary components. The results showed that observed S. album wood of a 46-year-old tree is diffuse-porous to semi-diffuse-porous wood. The maximum vessel tangential diameter is 127.47 μm, which is found at the beginning of the earlywood. The wood rays are heteromorphic type I and II, and the multi-column part is mostly 3 cells wide. In physical properties, the air-dry density is classified as “heavy”, whereas its air-dry and full-dry differential dry shrinkage are “small” and “medium”, respectively. This indicates that the wood performs better when dried. The content of benzene-ethanol extract from S. album wood is 2.10%. The benzene-ethanol extracts were analyzed by GC-MS, and the main components are 2,6,11,15-tetramethylhexadecane (3.29%), eicosamethyl cyclodecasiloxane (10.02%), octadecamethyl cyclononasiloxane (7.43%), and tetracosamethyl cyclododeca- siloxane (3.60%), etc.

Research on the structure and connections of pits in different cells of moso bamboo (Phyllostachys pubescens)

The plant grows within the transportation of water and nutrients, including radial and longitudinal, but bamboo only exists pits in the radial, so it plays an irreplaceable role at this moment. This study aims at giving rise to further understanding of the biological functions of pits in bamboo. Light microscopy (LM), scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were applied to investigate the structure and connections of bamboo pits. The results show that the arrangement of pits is significantly different, including alternate, scalariform and opposite arrangements. The presence or absence of the bordered on different cells is also displayed distinctively, these characteristics extremely affect the transportation of water and nutrients in bamboo.