CONTENTS
1. ANDRZEJ KRAUSS, WALDEMAR MOLIŃSKI, JOZEF KÚDELA, IGOR ČUNDERLÍK:
Differences in the mechanical properties of early and latewood within individual annual rings in dominant
pine tree (Pinus sylvestris L.) . 1
2. KHIN MAUNG SINT, HOLGER MILITZ, FRANTIŠEK HAPLA, STERGIOS ADAMOPOULOS:
Treatability and penetration indices of four lesser-used myanmar hardwoods . 13
3. VLADIMÍR GRYC, PETR HORÁČEK, JARMILA ŠLEZINGEROVÁ, HANUŠ VAVRČÍK:
Basic density of spruce wood, wood with bark, and bark of branches in locations in the czech republic . 23
4. THOMAS GEREKE, K. KRANITZ, KILIAN ANHEUSER, P. LEHMAN, PETER NIEMZ:
Moisture behaviour of recent and naturally aged wood . 33
5. MICHAL RYBNÍČEK, TOMÁŠ KOLÁŘ, EVA KOŇASOVÁ: Possibilities for dendrochronological
dating of large woody debris . 43
6. JACEK WILKOWSKI, JAROSŁAW GÓRSKI: Vibro-acoustic signals as a source of information about
tool wear during laminated chipboard milling . 57
7. DOMINIKA GORNIK BUČAR, BOJAN BUČAR: Strength grading of structural timber using the
single mode transverse damped vibration method . 67
8. ARNOLD WILCZYŃSKI, MAREK KOCISZEWSKI: Determination of elastic constants of
particleboard layers by compressing glued layer specimens . 77
9. ALBERT RUSS, MÁRIA FIŠEROVÁ: Estimation of hardwood species in mixture by near infrared
spectroscopy . 93
10. MURAT ÖZALP, SÜLEYMAN KORKUT: The research of borax pentahydrate effects with water-
based double components in varnish applicacions of wooden materials . 105
11. MARCIN KLIMCZEWSKI, DANUTA NICEWICZ: Influence of glucose and parameters of mat
pressing on the properties of mdf board . 115
12. VERENA KRACKLER, DANIEL KEUNECKE, PETER NIEMZ, ANDREAS HURST:
Possible fields of hardwood application . 125
13. RAMAZAN KURT, VEDAT CAVUS:
Manufacturing of parallel strand lumber (PSL) from rotary peeled hybrid poplar I-214 veneers with phenol
formaldehyde and urea formaldehyde adhesives . 137
14 GÜNTER SCHULZE-DEWITZ: SHORT NOTES - Some remarks about a famous Swedish
scientist . 145
Contents
Download WR201101 00 Contents
Download WR201101 01 Articles
Download WR201101 02 Articles
Download WR201101 03 Articles
Download WR201101 04 Articles
Download WR201101 05 Articles
Download WR201101 06 Articles
Download WR201101 07 Articles
Download WR201101 08 Articles
Download WR201101 09 Articles
Download WR201101 10 Articles
Download WR201101 11 Articles
Download WR201101 12 Articles
Download WR201101 13 Articles
Download WR201101 14 Articles