1. Xuexia Zhang, Yan Yu, Zehui Jiang, Hankun Wang: Influence of
thickness and moisture content on the mechanical properties of microfibrillated cellulose (MFC)
films . 851
2. Lenka Melzerová, Lucie Kucíková, Tomáš Janda, Michal
Šejnoha: Estimation of orthotropic mechanical properties of wood based on non-destructive
testing . . 861
3. Olena Pinchevska, Andriy Spirochkin, Ján Sedliačik,
Rostislav Oliynyk: Quality assessment of lumber after low temperature drying from
the view of stochastic process characteristics . 871
4. Alperen Kaymakci, Nadir Ayrilmis, Huseyin Akkilic: Utilization
of tinder fungus as filler in production of HDPE/wood composite 885
5. Roman Réh, Martin Guoth: Thermoplastic plywood and it’s drawback when
moderately heated . . . . . 895
6. Suleyman Ustun, Ergun Baysal, Turkay Turkoglu, Hilmi
Toker, Cevdet Sacli, Huseyin Peker: Surface characteristics of scots pine
treated with chemicals containing some copper compounds after weathering . . . 903
7. Juraj Gigac, Monika Stankovská, Andrej Pažitný: Influence of the
coating formulations and base papers on inkjet printability . . . 915
8. Birol Üner, Kenan Kömbeci, Mehmet Akgül: The utilization of tomato
stalk in fiber production: NAOH and CAO pulping process . . . . 927
9. Adam Wójciak: Deacidification of paper with Mg(OH)2 nanoparticles: The impact of dosage on
process effectiveness . . . 937
10. Bo-Han Xu, Yan-Hua Zhao, Jing-Hua Guo, Ya-Xun Wang: Fracture
toughnesses of interlaminar fracture of glued-laminated timber . . . 951
11. Onur Ülker, Erol Burdurlu: Some mechanical properties of densified and laminated
Lombardy poplar (Populus nigra L.) . . . 959
12. Xu Jiahe, Zhou Yucheng, Qi Yuhan, Hou Xiaopeng, Ge Zhedong,
Chen Yongping: A weighted filtered back projection algorithm for log CT two-dimensional and
three-dimensional image reconstruction . . . 971
13. Iveta Marková, Eva Mračková, Alena Očkajová, Juraj
Ladomerský: Granulometry of selected wood dust species of dust from orbital sanders 983
14. Ergün Güntekin, Tugba Yilmaz Aydin: Prediction of bending properties for some
softwood species grown in Turkey using ultrasound . . . 993
15. Martin Boldiš, Miroslav Gašparík, Milan Gaff, Daniel Ruman:
Compression set of PU foam mattresses with self-clamping joints and sandwich structure . . . 1003
16. Kaiting Zhang, Yuxia Chen, Yong Guo, Shengquan Liu,
Tingliang Guan, Na Su, Shiliu Zhu: Research of bamboo qualitative material tactile
characteristics . . . 1017
17. Jin Heon Kwon, Nadir Ayrilmis: Short note. Effect of hot-pressing parameters on selected
properties of flakeboard . . . 1033
Contents
Download WR201606 00 Contents
Download WR201606 01 Articles
Download WR201606 02 Articles
Download WR201606 03 Articles
Download WR201606 04 Articles
Download WR201606 05 Articles
Download WR201606 06 Articles
Download WR201606 07 Articles
Download WR201606 08 Articles
Download WR201606 09 Articles
Download WR201606 10 Articles
Download WR201606 11 Articles
Download WR201606 12 Articles
Download WR201606 13 Articles
Download WR201606 14 Articles
Download WR201606 15 Articles
Download WR201606 16 Articles
Download WR201606 17 Articles