1. ENHUA XI: Dynamic relationship between mechanical properties and chemical composition
distribution of wood cell walls . 179
2. GANIS LUKMANDARU: Chemical characteristics of Eucalyptus pellita with heart rot . 193
3. JÁN GÁPER, SVETLANA GÁPEROVÁ, TERÉZIA GAŠPARCOVÁ, SIMONA
KVASNOVÁ, PETER PRISTAŠ, KATEŘINA NÁPLAVOVÁ: Indoor fungal destroyers
of wooden materials – their identification in present review . 203
4. MAHARSHI J DAVE, TEJAS PANDYA, DAMIAN STODDARD, JASON
STREET, CODY BLAKE, PHONG LY: Dynamic and damping properties of novel
bio-composites using the hammer excitation vibration technique . 215
5. ZHIQIANG WANG, WEIQUN DONG, ZHUANZHUAN WANG, JIANHUI
ZHOU, MENG GONG: Effect of macro characteristics on rolling shear properties of
fast-growing poplar wood laminations . 227
6. SARA ESSERT, VERA REDE, ZRINKA ŠVAGELJ: The bending modulus of elasticity
of subfossil elm wood . 239
7. MINGBIN LIU, YOUFU SUN, CHEN SUN, XIAOLIN YANG: Study on thermal
insulation and heat transfer properties of wood frame walls . 249
8. HORÁK JIŘÍ, KUBOŇOVÁ LENKA, TOMŠEJOVÁ ŠÁRKA, LACIOK
VENDULA, KRPEC KAMIL, HOPAN FRANTIŠEK, KUBESA PETR,
KYSUČAN ZDENĚK, OCHODEK TADEÁŠ: Change in the wood moisture dependency
on time and drying conditions for heating by wood combustion . 261
9. HERVICE KOUEFOUET, G. BAWE, C.M. FOUOTSA WOUTSOP, P. K. TALLA,
J.A. MUKAM FOTSING, E. FOADIENG: Probabilistic approach of the failure of Lovoa trichilioides
and Triplochiton scleroxylon . 273
10. LISHU WANG, SHENGBO GE, DONGLI LI, WEI YANG, WANXI PENG:
Characteristics of nontoxic bamboo bioboard by melamine and cellulose adhesive . 287
11. MARIUSZ RECZULSKI: Optimization of the clearance angle in industrial disc chipper . 295
12. JIAYU CONG, GUOCHAO YANG, LIJUAN ZHAO, QIUHUI ZHANG:
The synergistic smoke suppression effect of ferric oxide on flame retardant wood-polyurethane
composites . 305
13. WIESŁAW FRĄCZ, GRZEGORZ JANOWSKI: Determination of viscosity curve
and PVT properties for wood-polymer composite . 321
14. LINGLING HUANG, HUIYUN WANG, XIAOLEI GUO, ZHIHUA JIANG, FENG
XING, LINGLING HUANG, MATS EKEVAD: Study on continuous cold-pressing
technology of engineered wood flooring with EPI adhesive . 335
15. MURAT KILIÇ, INCI PÜRLUSOY, MELIH KURNALI: Measuring the surface roughness
values of european hop-horn beam (Ostrya carpinifolia Scop.) wood . 343
16. ZHI LIU, JINZHEN CAO: Fabrication of superhydrophobic wood surface with a silica/silicone oil
complex emulsion . 353
Contents
Download WR201802 00 Contents
Download WR201802 01 Articles
Download WR201802 02 Articles
Download WR201802 03 Articles
Download WR201802 04 Articles
Download WR201802 05 Articles
Download WR201802 06 Articles
Download WR201802 07 Articles
Download WR201802 08 Articles
Download WR201802 09 Articles
Download WR201802 10 Articles
Download WR201802 11 Articles
Download WR201802 12 Articles
Download WR201802 13 Articles
Download WR201802 14 Articles
Download WR201802 15 Articles
Download WR201802 16 Articles