WR2020 03: 01-15 WR 202003
Contents:download1. DARIUS ALBREKTAS, MILDA JUCIENĖ, VAIDA DOBILAITĖ:The influence of thermal modification on the resistance to water impact properties and strength of wood used in outdoor conditions. 353doi.org/10.37763/wr.1336-4561/65.3.3533642. SHEIKH ALI AHMED, STERGIOS ADAMOPOULOS, FRANCESCO POGGI, THOMAS WALTHER:Resonance and time-of-flight methods for evaluating the modulus of elasticity of particleboards at different humid conditions. 365doi.org/10.37763/wr.1336-4561/65.3.3653803. RUYUAN YANG, XIAOFENG ZHANG, YOUFU SUN, TINGTING ZHOU, QUAN YUAN:Effect of the metallization treatment on the surface properties of Populus euphratica. 381doi.org/10.37763/wr.1336-4561/65.3.3813944. CANDAN KUS SAHIN, MEHMET TOPAY, AHMET ALI VAR:A study on suitability of some wood species for landscape applications: Surface color, hardness and roughness changes at outdoor conditions. 395doi.org/10.37763/wr.1336-4561/65.3.3954045. ADAM KRAJEWSKI, PAWEŁ KOZAKIEWICZ, PIOTR WITOMSKI:Comparison of selected properties of natural aged wood and contemporary timber of Pinus sylvestris L. investigated using standard methods and measuring of transition speed of ultrasounds along the fibre. 405doi.org/10.37763/wr.1336-4561/65.3.4054146. MENGPEI LIU, QINGXIN DU, PANFENG LIU, JUN QING, HONGYAN DU, LU WANG:Characterization of new mutant Eucommia ulmoides constituents in the discoloration during growing. 415doi.org/10.37763/wr.1336-4561/65.3.4154227. MATEJ HOLC, IGOR KARLOVITS, DAVID RAVNJAK, ALEŠ PALATINUS, ITA JUNKAR:Influence of gaseous plasma treatment on functional properties of coated papers. 423doi.org/10.37763/wr.1336-4561/65.3.4234368. IVANA PLAZONIĆ, ŽELJKA BARBARIĆ-MIKOČEVIĆ, NIKOLA ŠPANIĆ:Effect of agricultural residue fibers on newsprint strength properties. 437doi.org/10.37763/wr.1336-4561/65.3.4374469. MONIKA STANKOVSKÁ, MÁRIA FIŠEROVÁ, JURAJ GIGAC, ELENA OPÁLENÁ:Blending impact of hardwood pulps with softwood pulp on tissue paper properties. 447doi.org/10.37763/wr.1336-4561/65.3.44745810. YULAI YANBAEV, RIDA SULTANOVA, LIUBOV BLONSKAYA, SVETLANA BAKHTINA, ALBINA TAGIROVA, VADIM TAGIROV, ALEKSEY KULAGIN:Gene pool of Scots pine (Pinus sylvestris L.) under reforestation in extreme environmen. 459doi.org/10.37763/wr.1336-4561/65.3.45947011. PEIXING WEI, WANYONG TUO, SHENG HE, GUOHUA LIU:Heat-induced inkless eco-printing inspired by paper discoloration: A review. 471doi.org/10.37763/wr.1336-4561/65.3.47148412. NURDAN CETIN YERLIKAYA, ABDURRAHMAN KARAMAN:Effect of the fabric reinforcement of structural holes in wood based panels. 485doi.org/10.37763/wr.1336-4561/65.3.48549613. WEN-GANG HU, NA LIU, LU XU, HUIYUAN GUAN:Study on cold/warm sensation of materials used in desktop of furniture. 497doi.org/10.37763/wr.1336-4561/65.3.49750614. NIKOLA VELIMIROVIĆ, IVAN STANIMIROVIĆ, DRAGOSLAV STOJIĆ, NEMANJA MARKOVIĆ, MILIVOJE MILANOVIĆ:Economical design of timber-concrete composite beams. 507doi.org/10.37763/wr.1336-4561/65.3.50752015. ESRA CELIK, ISMAIL CENGIZ YILMAZ, DENIZ YILMAZ:An experimental study on sustainability of historical wooden buildings exposed to open sea streams. 521doi.org/10.37763/wr.1336-4561/65.3.521530 |