EVALUATION OF SELECTED MECHANICAL AND PHYSICAL PROPERTIES OF PARTICLEBOARDS CONTAINING WASTE PLASTICS

This article is focused on the research of particleboards (PB) composed of wood particles from spruce logs and recycled crushed plastic granulates. Crushed plastic granulates sized from 1.0 to 4.0 mm were obtained from worn automobiles by recycling, specifically painted and unpainted bumpers. The proportion of plastic granulate in the particleboards represented 10%, 15%, and 20% of the total weight of the composites. In the production of PB, urea-formaldehyde resin and paraffin emulsion were used as a binder and ammonium nitrate was used as a hardener. The aim of the article was to compare the selected properties of PB containing plastic filler with pure PB. Mechanical properties (tensile and bending strength), and physical properties (water absorption and thickness swelling) were evaluated according to EN 319, EN 310 and EN 317. Based on the results, it can be stated that the bending strength and physical properties of PB containing plastic filler were significantly better compared to pure PB. On the contrary, the tensile strength values were lower in most cases

Thermoplastic plywood and it’s drawback when moderately heated

GradaTM is new plywood which contains the thermoplastic adhesive. There are so far two material versions 1000 and 2000 which have wide potential in production of wooden products with new perspective of manufacturing. This paper investigates possibilities of including GradaTM material and its versions in skateboard production. Bending strengths at the moderate heat up of this material are presented, specifically at 30, 40°C for both material versions. All increased temperatures are compared to the room temperature (20°C). Mechanical properties that were obtained from the test are modulus of elasticity, modulus of rapture, and stroke strain. The results show the undesirable level of changes present in both versions however version 1000 acts significantly better than 2000.