Tackiness reducing of the stickies surfaces by inorganic agents and organic polymers

This paper present the results of application of inorganic minerals and organic polymers for elimination of sticky impurities “macrostickies” in the processing of recovered paper. The impact of individual agents has been monitored on different species of suspensions. On the dark suspension of recycled fibres VL5 with a brightness 53% ISO and an ash content of 17.6%, and the suspension VL1 with a brightness 64% ISO and an ash content of 29.4%. From inorganic minerals, the highest efficiency was achieved in the elimination of macrostickies using bentonite Hydrocol OT. At a dose of 5 kg bentonite.t-1 b.d. recycled fibres efficiency of 65.1% for suspension VL5 and 58.7% for VL1 was achieved. The highest performance of the Acefloc 2550 was achieved from the polymers. When applied to the VL5 suspension, the macrostickies were reduced by 57.1%, and when applied to the VL1 suspension, the macrostickies content dropped by 56.5%.

Elimination of adhesive impurities of the recovered paper in flotation process

The article presents results of the elimination of sticky impurities from recovered paper in laboratory flotation of three pulp suspensions with different whiteness, obtained directly from the production line before entering flotation. A combination of commercial agents releasing undesirable substances from recovered paper and means for regulation and stabilization of froth and modified micronized bentonit was used. In the flotation purification of pulp suspension with a whiteness of 53%, the combination of Prodeink Extra, Prodeink AS10 and Hydrocol OT reduced the macrostickies content by 58%, the ash content decreased from 18.5% to 4.5%, the whiteness increased from 53% to 56.4% and the residual color content was reduced from 385 ppm to 294 ppm. The pulp suspension with a whiteness of 64% showed a reduction in the content of macrostickies by 66%, a reduction in the ash content by 23.2%, an increase in whiteness by 1.4% and a reduction in the residual color content from 245 ppm to 194 ppm. The pulp suspension with a whiteness of 68.3% showed a decrease in the content of macrostickies by 58.1%, the ash content decreased from 35.7% to 6.3%, the whiteness increased by 1.1% and the content of residual color decreased from 157 ppm to 117 ppm.